Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ASTM D257 |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ASTM D257 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ASTM D257 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ASTM-D257 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Surface Resistance | 3.20e+13 ohm | 3.20e+13 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c.. |