Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.2e+9 - 3.2e+10 ohm | 3.2e+9 - 3.2e+10 ohm | IS 3396-1979 |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |