Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.80e+12 ohm | 3.80e+12 ohm | ASTM D257 |
Shell Carilon® DP R1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi.. |