Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.00e+11 ohm | 4.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 225F PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Surface Resistance | 4.00e+11 ohm | 4.00e+11 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management. |
|||
Surface Resistance | 4.00e+11 ohm | 4.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 208F PA66, Conditioned Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |