Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.62e+14 ohm | 6.62e+14 ohm | IEC 93 |
Polycasa COPOL PETG QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v.. |
|||
Surface Resistance | 6.62e+14 ohm | 6.62e+14 ohm | IEC 93 |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |