Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 800 ohm | 800 ohm | |
LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled Dissipative product based on Polypropylene homopolymer (PPh). Mica filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |