Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 9.00e+13 ohm | 9.00e+13 ohm | IEC 60093 |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Surface Resistance | 9.00e+13 ohm | 9.00e+13 ohm | ASTM D257 |
CRP Technology Windform® FX Polyamide Composite Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive.. |
|||
Surface Resistance | 9.00e+13 ohm | 9.00e+13 ohm | E24/125; IPC TM-650 2.5.17.1 |
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg 85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia.. |