Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+14 ohm-cm

@Temperature 65.6 °C
5.00e+14 ohm-cm

@Temperature 150 °F
Abatron AboCast 8-14/Abocure 8-14 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.10 ratio (pbw); Gel time, 100 g (3.5 oz.): 63 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..