Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5.00e+14 ohm-cm @Temperature 65.6 °C |
5.00e+14 ohm-cm @Temperature 150 °F |
|
Abatron AboCast 8-14/Abocure 8-14 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.10 ratio (pbw); Gel time, 100 g (3.5 oz.): 63 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |