Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 7.10e+12 ohm @Temperature 23.0 °C |
7.10e+12 ohm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |