Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 220 V | 220 V | ASTM D3638 |
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
Comparative Tracking Index | 220 V | 220 V | IEC Tracking Index |
Sumitomo Bakelite Durez® 25378 Phenolic, Compression Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Comparative Tracking Index | 220 V | 220 V | IEC Tracking Index |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Comparative Tracking Index | 220 V | 220 V | IEC test |
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt.. |
|||
Comparative Tracking Index | 220 V | 220 V | IEC test |
Toyobo Vylopet® EMC130-04 Glass Reinforced Polyester, Easy Molding Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking r.. |
|||
Comparative Tracking Index | 220 V | 220 V | |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Comparative Tracking Index | 220 V | 220 V | IEC test |
Toyobo Vylopet® EMC615 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Comparative Tracking Index | 220 V | 220 V | IEC test |
Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trackin.. |
|||
Comparative Tracking Index | 220 V | 220 V | UL 746A |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |