Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.0021 ohm @Thickness 0.0180 mm, Temperature 850 °C |
0.0021 ohm @Thickness 0.000709 in, Temperature 1560 °F |
|
Gwent Electronic Materials C2050303D1 Fine Line Printing Ink Silver Ink has been designed for fine line printing. It is capable of printing down to 50 micron line and spaces within a production environment. Under laboratory conditions, finer lines and spaces .. |
|||
Surface Resistivity per Square | 0.0021 ohm | 0.0021 ohm | fired; 18 microns thick |
Gwent Electronic Materials C2010515D4 Silver Ink Silver Ink C2010515D4 is designed as an internal electrode ink for LTCC applications. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the mark.. |