Gwent Electronic Materials C2050303D1 Fine Line Printing Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2050303D1 Fine Line Printing Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silver Ink has been designed for fine line printing. It is capable of printing down to 50 micron line and spaces within a production environment. Under laboratory conditions, finer lines and spaces have been produced. The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers. Screen Printing Equipment: semi-automatic, automaticScreen Types: stainless steel, polyester, mesh 156-325 tpiSubstrate: Polyester, PVC, Polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 69 - 71 %

@Temperature 700 °C
69 - 71 %

@Temperature 1290 °F
Viscosity 14000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
14000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.0021 ohm

@Thickness 0.0180 mm,
Temperature 850 °C
0.0021 ohm

@Thickness 0.000709 in,
Temperature 1560 °F
Processing Properties Metric English Comments
Sintering Temperature >= 700 °C
>= 1290 °F
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
15.0 min

@Temperature 120 °C
0.250 hour

@Temperature 248 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 80
Using a 230 mesh stainless steel screen