Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | [ohm/in<sup>2<sup>]; <.0016 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FOIL CCD Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | [ohm/in<sup>2<sup>]; <.0016 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FOIL CCJ Shielding Tape Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or .. |
|||
Surface Resistivity per Square | 0.010 ohm | 0.010 ohm | Initial, 2190 hours @ 158°F; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 5500 EMI Shielding and Grounding Gasket SOFT-SHIELD 5500 EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electronics, factory automatio.. |
|||
Surface Resistivity per Square | 0.010 ohm | 0.010 ohm | Final, 2190 hours @ 158°F; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 5500 EMI Shielding and Grounding Gasket SOFT-SHIELD 5500 EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electronics, factory automatio.. |
|||
Surface Resistivity per Square | 0.010 ohm | 0.010 ohm | |
Lord Adhesives Metech 3502 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | |
Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound AboCoat 8401-1 A/B is a conventional highly-filled coating to produce conductive paths with the highest silver content possible. It requires strict controls. Resistivity may rise to 0.1 ohm/sq under.. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | |
Abatron AboCoat 8709-10 Silver-Filled Electrically Conductive Acrylic Compound AboCoat 8709-10 is a high-grade silver-acrylic 1-component coating that needs no A/B mixing. It is excellent where the epoxy adhesion and thermochemical properties are not needed. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | |
Abatron AboCoat 8709-12/AboCure 50-12 Silver-Filled Electrically Conductive Epoxy Compound AboCoat 8709-12/AboCure 50-12 is a versatile silver-epoxy high-solids coating with good conductive and adhesive properties. It is successful as a conductive compound for most electronic uses. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | |
Abatron AboWeld 8201-14/AboCure 8201-14 Carbon-Filled Electrically Conductive Epoxy Compound AboWeld 8201-14/AboCure 8201-14 is an easy-to-use and very conductive carbon-epoxy paste. As the size of the conductive particles is relatively coarse, this product is used primarily as a thick adhe.. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | |
Abatron AboWeld 8505-1 A/B Silver-Filled Electrically Conductive Epoxy Compound AboWeld 8505-1 A/B is a solventless silver-epoxy adhesive and resurfacer. It has high rigidity, chemical and heat resistance. It also has good adhesion to most rigid materials. |
|||
Surface Resistivity per Square | <= 0.010 ohm | <= 0.010 ohm | [ohm/in<sup>2<sup>]; <.0016 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FOIL CAD Shielding Tape Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or .. |