Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboWeld 8201-14/AboCure 8201-14 Carbon-Filled Electrically Conductive Epoxy Compound

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer Abatron
Trade Name AboWeld
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboWeld 8201-14/AboCure 8201-14 Carbon-Filled Electrically Conductive Epoxy Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboWeld 8201-14/AboCure 8201-14 is an easy-to-use and very conductive carbon-epoxy paste. As the size of the conductive particles is relatively coarse, this product is used primarily as a thick adhesive and conductive paste rather than for thin and smooth coatings.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Component Elements Properties Metric English Comments
Carbon, C 69 %
69 %
of vehicle
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.010 ohm
<= 0.010 ohm
Processing Properties Metric English Comments
Cure Time 30.0 - 180 min

@Temperature 50.0 - 100 °C
0.500 - 3.00 hour

@Temperature 122 - 212 °F
Optional
>= 1440 min

@Temperature 22.0 - 30.0 °C
>= 24.0 hour

@Temperature 71.6 - 86.0 °F
Pot Life 200 min
200 min
Descriptive Properties Value Comments
Color Black
Parts by Weight (pbw) 100
AboWeld 8201-14
50
AboCure 8201-14
Viscosity Paste