Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.040 ohm @Temperature 150 °C |
0.040 ohm @Temperature 302 °F |
Alumina substrate dried at 150°C for 30 min |
Gwent Electronic Materials C2100203D2 Silver Ink This product is part of a range of Heat Curable Inks. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has exce.. |
|||
Surface Resistivity per Square | 0.040 ohm @Temperature 200 °C |
0.040 ohm @Temperature 392 °F |
Cured Film at 200°C for 30 min |
Gwent Electronic Materials C2100211D1 Silicone Based Silver Paste This ink can be used in a wide range of applications, as conductive adhesive, it has excellent chemical resistance, with good adhesion. This product has been tested at 250°C and it showed good s.. |
|||
Surface Resistivity per Square | <= 0.040 ohm @Thickness 508 mm |
<= 0.040 ohm @Thickness 20.0 in |
|
Parker Chomerics CHO-SHIELD® 2052 Conductive Coating CHO-SHIELD® 2052 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |