Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gwent Electronic Materials C2100203D2 Silver Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2100203D2 Silver Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is part of a range of Heat Curable Inks. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties.Excellent adhesion to ITOScreen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156 to 325tpiSubstrate: ITO coated polyester, alumina, polyesterInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 57 - 59 %

@Temperature 700 °C
57 - 59 %

@Temperature 1290 °F
Viscosity 6500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
6500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 32.0 microns
1.26 mil
On alumina substrate
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Volume Resistivity 0.00040 ohm-cm
0.00040 ohm-cm
On glass slide dried at 150°C for 30 min
Surface Resistivity per Square 0.040 ohm

@Temperature 150 °C
0.040 ohm

@Temperature 302 °F
Alumina substrate dried at 150°C for 30 min
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
30.0 min

@Temperature 180 °C
0.500 hour

@Temperature 356 °F
box oven
60.0 min

@Temperature 130 °C
1.00 hour

@Temperature 266 °F
box oven
Shelf Life 6.00 Month
6.00 Month