Polymer Property : Surface Resistivity per Square = 0.050 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.050 ohm
<= 0.050 ohm
Parker Chomerics CHO-SHIELD® 4900 Conductive Coating
CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Fil..
Surface Resistivity per Square <= 0.050 ohm
<= 0.050 ohm
Typically
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket
Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance ..
Surface Resistivity per Square <= 0.050 ohm

@Thickness 0.0254 mm
<= 0.050 ohm

@Thickness 0.00100 in
film
Parker Chomerics CHO-FLEX 601 Conductive Coating
CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adh..
Surface Resistivity per Square <= 0.050 ohm
<= 0.050 ohm
Lord Adhesives 6100 Silver Conductor
LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di..
Surface Resistivity per Square <= 0.050 ohm
<= 0.050 ohm
Parker Chomerics CHO-SHIELD® 2052 Conductive Coating
CHO-SHIELD® 2052 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo..
Surface Resistivity per Square <= 0.050 ohm
<= 0.050 ohm
ASTM F390
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric
P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave ..