Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+10 ohm | >= 1.00e+10 ohm | ASTM D257 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+10 ohm | >= 1.00e+10 ohm | ASTM D257 |
Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+10 ohm | >= 1.00e+10 ohm | VDE 0303 |
GEHR Plastics PA 6 Nylon 6, Conditioned Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D648 |
Techmer ES Electrafil® ABS-1200/SD/FR BL ABS |
|||
Surface Resistivity per Square | <= 1.00e+10 ohm | <= 1.00e+10 ohm | ASTM D257 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Surface Resistivity per Square | <= 1.00e+10 ohm | <= 1.00e+10 ohm | ASTM D257 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Surface Resistivity per Square | 1.00e+10 ohm | 1.00e+10 ohm | ASTM D257 |
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an in.. |
|||
Surface Resistivity per Square | 1.00e+10 ohm @Temperature 20.0 °C |
1.00e+10 ohm @Temperature 68.0 °F |
500 V DC @ 60% RH; ASTM D257 |
DuPont Teijin Films Melinex® 539 Polyester Film, 370 Gauge Melinex® 539 is a two sided treated grade of clear film for applications where freedom from static is required. Its main use is as a montage "foil" in the production of printing plates. Melinex® 5.. |
|||
Surface Resistivity per Square | 1.00e+10 ohm | 1.00e+10 ohm | Non-adhesive side; ASTM D257 |
3M 4516 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |