Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech 513 Static Dissipative Control Sheet

Category Polymer , Thermoplastic
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech 513 Static Dissipative Control Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Static Control SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D638
Flexural Yield Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Unnotched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1.00e+10 ohm
<= 1.00e+10 ohm
ASTM D257
Users viewing this material also viewed the following: