Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
Ovation Polymers OpteSTAT™ NC PES 6010 Polyether Sulfone based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Surface Resistivity per Square | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
Ovation Polymers OpteSTAT™ NC PK 8010 Polyetheretherketone based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Surface Resistivity per Square | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
Ovation Polymers OpteSTAT™ NC TPU 9020 Polyurethane-based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Surface Resistivity per Square | 10000 - 1.00e+7 ohm @Temperature 23.0 °C |
10000 - 1.00e+7 ohm @Temperature 73.4 °F |
50% RH; ASTM D250 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Surface Resistivity per Square | 10000 - 1.00e+7 ohm @Temperature 23.0 °C |
10000 - 1.00e+7 ohm @Temperature 73.4 °F |
50% RH; ASTM D250 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |