Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers OpteSTAT™ NC TPU 9020 Polyurethane-based Carbon Nanotube Compound

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced
Manufacturer Ovation Polymers
Trade Name OpteSTAT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers OpteSTAT™ NC TPU 9020 Polyurethane-based Carbon Nanotube Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or other electronic assemblies where ESD control is required while retaining exceptional cleanliness, dimensional control and physical propertiesAll properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.00 MPa
1020 psi
50 mm/min; ASTM D638
Elongation at Yield 6.5 %
6.5 %
50 mm/min; ASTM D638
Izod Impact, Notched 0.481 J/cm

@Temperature 23.0 °C
0.900 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 10000 - 1.00e+7 ohm
10000 - 1.00e+7 ohm
ASTM D257
Users viewing this material also viewed the following: