Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
ASTM D955
Melt Flow <= 1.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
<= 1.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 100 %
100 %
chs 2.0 in/min; ASTM D638
Flexural Strength 34.4 MPa
4990 psi
ASTM D790
Flexural Modulus 2.274 GPa
329.8 ksi
ASTM D790
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 59.4 µm/m-°C
33.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05 - 1.00e+7 ohm-cm
1e+05 - 1.00e+7 ohm-cm
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257