Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | |
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+9 ohm | 1e+05 - 1.00e+9 ohm | |
NeXolve LaRC™-CP1 Conductive Black Polyimide Lower RF loss than other black and conductive black polyimides. NeXolve’s Conductive Black LaRC™-CP1 Polyimide is filled with carbon nanoparticles to produce a conductive black polyimide material .. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+9 ohm | 1e+05 - 1.00e+9 ohm | ASTM D257 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+9 ohm | 1e+05 - 1.00e+9 ohm | ASTM D257 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1003 PS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+9 ohm | 1e+05 - 1.00e+9 ohm | |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT R048BK PS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT R048BK PS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1000 PC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | after 250% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1000 PC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Ensinger Tecaform™ SD Acetal (POM) Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent b.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+14 ohm | 1.00e+9 - 1.00e+14 ohm | ASTM D257 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Surface Resistivity per Square | 1.00e+9 ohm | 1.00e+9 ohm | IEC 60093 |
Arkema Group Pebax® MH 1657 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MH 1657 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 1657 is an inherently dissipative polymer and can be dry blended or compounded w.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+12 ohm | 1.00e+9 - 1.00e+12 ohm | ASTM D257 |
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet
(discontinued **) Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT P048BK PP Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |