Material Notes:
Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent bearing and wear characteristics, TECAFORM™ SD is ideal for moving components which may experience frictional or fluid-flow static charges.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Water Absorption 0.20 %

@Temperature 22.8 °C,
Time 86400 sec
0.20 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.18

@Pressure 0.276 MPa
0.18

@Pressure 40.0 psi
50 fpm
Coefficient of Friction, Static 0.11

@Pressure 0.276 MPa
0.11

@Pressure 40.0 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Descriptive Properties Value Comments
Base Material Acetal