Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 5.00e+13 ohm

@Temperature 25.0 °C
5.00e+13 ohm

@Temperature 77.0 °F
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite
MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi..