Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 5.00e+13 ohm @Temperature 25.0 °C |
5.00e+13 ohm @Temperature 77.0 °F |
|
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi.. |