Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Resistivity per Square = 63 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 63 ohm
63 ohm
Typical, Printed through 230 stainless steel mesh with 13 micron emulsion
Gwent Electronic Materials C2030408P3 Carbon Graphite Ink
This product is designed to be used for screen printing working electrodes. This is a carbon/graphite ink which has been optimized to give superior electrochemical performance and contains Cobalt Ph..