Material Notes:
This product is designed to be used for screen printing working electrodes. This is a carbon/graphite ink which has been optimized to give superior electrochemical performance and contains Cobalt Phthalocyanine as mediator that makes it suitable for use with oxidase enzymes where hydrogen peroxide is generated and detected. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-230tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 39 - 42 %

@Temperature 130 °C
39 - 42 %

@Temperature 266 °F
Viscosity 2200 - 4300 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
2200 - 4300 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 12.0 microns
0.472 mil
Cured, Typical, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 63 ohm
63 ohm
Typical, Printed through 230 stainless steel mesh with 13 micron emulsion
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 80.0 °C
0.250 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 220
Using a 230 mesh stainless steel screen