Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 80.0 sec Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Arc Resistance | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 86.7 sec Grade Count:6 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Arc Resistance | 0.000 - 180 sec | 0.000 - 180 sec | Average value: 119 sec Grade Count:41 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Arc Resistance | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 96.5 sec Grade Count:15 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Arc Resistance | 0.000 - 180 sec | 0.000 - 180 sec | Average value: 111 sec Grade Count:29 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Arc Resistance | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 81.9 sec Grade Count:5 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Arc Resistance | 0.000 - 180 sec | 0.000 - 180 sec | Average value: 126 sec Grade Count:130 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |