Polymer Property : Arc Resistance = 159 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 159 sec
159 sec
ASTM D495
Plenco 3509 Phenolic, Granular, Transfer Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Arc Resistance 159 sec
159 sec
ASTM D495
Plenco 4599 Phenolic, Granular, Injection Molded
PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated ..
Arc Resistance 159 sec
159 sec
ASTM D495
Plenco 4311 Phenolic, Granular, Injection Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Arc Resistance 159 sec
159 sec
ASTM D495
Plenco 6500 Phenolic, Briquette, Injection Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..
Arc Resistance 159 sec
159 sec
ASTM D495
Plenco 7476 Phenolic, Granular, Transfer Molded
PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. ..