Polymer Property : Arc Resistance = 162 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 162 sec
162 sec
ASTM D495
Plenco 4414 Phenolic, Granular, Transfer Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..
Arc Resistance 162 sec
162 sec
ASTM D495
Plenco 6527 Phenolic, Granular, Transfer Molded
PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco.