Electrical Properties Metric English Comments
Arc Resistance 179 sec
179 sec
ASTM D495
Plenco 7507 Phenolic, Granular, Transfer Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Arc Resistance 179 sec
179 sec
ASTM D495
Plenco 7591 Phenolic, Pellet, Transfer Molded
PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.