Electrical Properties Metric English Comments
Arc Resistance 190 - 195 sec
190 - 195 sec
ASTM D495
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage  (dis
Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l..