Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 224 sec | 224 sec | ASTM D495 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |