Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 34 sec | 34 sec | |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |