Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 85.0 - 125 sec | 85.0 - 125 sec | Average value: 109 sec Grade Count:8 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |