Polymer Property : Arc Resistance = 95.0 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 95.0 - 185 sec
95.0 - 185 sec
Average value: 127 sec Grade Count:6
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..