Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 151 - 185 sec | 151 - 185 sec | Average value: 173 sec Grade Count:15 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Arc Resistance | 48.0 - 185 sec | 48.0 - 185 sec | Average value: 152 sec Grade Count:13 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Arc Resistance | 130 - 185 sec | 130 - 185 sec | Average value: 173 sec Grade Count:28 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Arc Resistance | 15.0 - 185 sec | 15.0 - 185 sec | Average value: 103 sec Grade Count:3 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Arc Resistance | 120 - 185 sec | 120 - 185 sec | Average value: 155 sec Grade Count:3 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Arc Resistance | 95.0 - 185 sec | 95.0 - 185 sec | Average value: 127 sec Grade Count:6 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |