Polymer Property : Static Decay = 0.30 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Static Decay 0.30 sec
0.30 sec
(Mil-B-81705C), 12% RH, 5000 kV to 50 kV
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Static Decay 0.30 sec
0.30 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene
Stat-Rite® X-5076 is a static dissipative, High Impact Polystyrene alloy. Stat-Rite® X-5076 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, p..
Static Decay <= 0.30 sec
<= 0.30 sec
15% RH; MIL-B-81705-B
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static)
Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th..
Static Decay <= 0.30 sec
<= 0.30 sec
15% RH; MIL-B-81705-B
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static)
Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac..
Static Decay <= 0.30 sec
<= 0.30 sec
15% RH; MIL-B-81705-B
Westlake Plastics Propylux® SD-A Polypropylene (anti-static)
Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, availab..
Static Decay 0.30 sec
0.30 sec
+5000 to 50 V; (12% R.H.); FTMS-101C
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound
Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm..