Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 0.40 sec | 0.40 sec | (Mil-B-81705C), 12% RH, 5000kV to 50kV |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |