Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | -7.00 dB @Frequency 2.30e+8 Hz |
-7.00 dB @Frequency 2.30e+8 Hz |
With wire ground termination |
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | -7.00 dB @Frequency 230 Hz |
-7.00 dB @Frequency 230 Hz |
|
Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | -7.00 dB @Frequency 2.70e+8 Hz |
-7.00 dB @Frequency 2.70e+8 Hz |
Jacketing terminated with wires only |
Parker Chomerics CHO-JAC® CJ-022 Flat Cable EMI Shield Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight .. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 2.36 mm, Frequency 1.05e+10 Hz |
-7.00 dB @Thickness 0.0930 in, Frequency 1.05e+10 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 0.813 mm, Frequency 1.55e+10 Hz |
-7.00 dB @Thickness 0.0320 in, Frequency 1.55e+10 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 1.57 mm, Frequency 5.00e+9 Hz |
-7.00 dB @Thickness 0.0620 in, Frequency 5.00e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 1.57 mm, Frequency 5.50e+9 Hz |
-7.00 dB @Thickness 0.0620 in, Frequency 5.50e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 2.36 mm, Frequency 1.55e+10 Hz |
-7.00 dB @Thickness 0.0930 in, Frequency 1.55e+10 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Frequency 2.70e+8 Hz |
-7.00 dB @Frequency 2.70e+8 Hz |
Jacketing terminated with wires only |
Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight .. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 2.36 mm, Frequency 1.05e+10 Hz |
-7.00 dB @Thickness 0.0930 in, Frequency 1.05e+10 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 2.36 mm, Frequency 1.55e+10 Hz |
-7.00 dB @Thickness 0.0930 in, Frequency 1.55e+10 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 1.57 mm, Frequency 5.00e+9 Hz |
-7.00 dB @Thickness 0.0620 in, Frequency 5.00e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 1.57 mm, Frequency 5.50e+9 Hz |
-7.00 dB @Thickness 0.0620 in, Frequency 5.50e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 1.57 mm, Frequency 6.80e+9 Hz |
-7.00 dB @Thickness 0.0620 in, Frequency 6.80e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -7.00 dB @Thickness 3.17 mm, Frequency 4.80e+9 Hz |
-7.00 dB @Thickness 0.125 in, Frequency 4.80e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |