Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 45.5 dB @Frequency 1.00e+6 Hz |
45.5 dB @Frequency 1.00e+6 Hz |
H-Field, Magnetic |
P & P Technology BS3075 NA13 Monel Wire Alloy 400L Wire Diameter 0.11mmInformation provided by P & P Technology |