Polymer Property : Shielding Effectiveness = 45.5 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 45.5 dB

@Frequency 1.00e+6 Hz
45.5 dB

@Frequency 1.00e+6 Hz
H-Field, Magnetic
P & P Technology BS3075 NA13 Monel Wire
Alloy 400L Wire Diameter 0.11mmInformation provided by P & P Technology