Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 76 dB @Frequency 1.00e+9 Hz |
76 dB @Frequency 1.00e+9 Hz |
P-Field |
P & P Technology Aluminum 5056 (AMS 4182) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | 76 dB @Frequency 200000 Hz |
76 dB @Frequency 200000 Hz |
H-Field |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Shielding Effectiveness | 76 dB @Frequency 1.00e+9 Hz |
76 dB @Frequency 1.00e+9 Hz |
P-Field |
P & P Technology Stainless Steel (Alloy 304) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | 76 dB @Frequency 1.00e+7 Hz |
76 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit SC-Consil® 862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 76 dB @Frequency 1.00e+7 Hz |
76 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit SC-Consil® 864 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |