Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

P & P Technology Stainless Steel (Alloy 304) Knitted Cored Shielding Mesh

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer P & P Technology
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology Stainless Steel (Alloy 304) Knitted Cored Shielding Mesh.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product has a diameter of 0.11mm.Information provided by P & P Technology
Electrical Properties Metric English Comments
Shielding Effectiveness 40 dB

@Frequency 10000 Hz
40 dB

@Frequency 10000 Hz
H-Field
44 dB

@Frequency 100000 Hz
44 dB

@Frequency 100000 Hz
H-Field
58 dB

@Frequency 1.00e+6 Hz
58 dB

@Frequency 1.00e+6 Hz
H-Field
60 dB

@Frequency 1.00e+10 Hz
60 dB

@Frequency 1.00e+10 Hz
P-Field
76 dB

@Frequency 1.00e+9 Hz
76 dB

@Frequency 1.00e+9 Hz
P-Field
94 dB

@Frequency 4.00e+8 Hz
94 dB

@Frequency 4.00e+8 Hz
P-Field
100 dB

@Frequency 1.00e+8 Hz
100 dB

@Frequency 1.00e+8 Hz
E-Field
120 dB

@Frequency 1.00e+7 Hz
120 dB

@Frequency 1.00e+7 Hz
E-Field
125 dB

@Frequency 1.00e+6 Hz
125 dB

@Frequency 1.00e+6 Hz
E-Field