Electrical Properties Metric English Comments
Shielding Effectiveness 83 - 93 dB

@Frequency 1.00e+9 Hz
83 - 93 dB

@Frequency 1.00e+9 Hz
Parker Chomerics COMBO® and COMBO® Strip Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel ..
Shielding Effectiveness 83 - 93 dB

@Frequency 1.00e+9 Hz
83 - 93 dB

@Frequency 1.00e+9 Hz
Parker Chomerics MESH STRIP™ (all metal) Wire Mesh EMI Gasket Selection Guide
Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by C..
Shielding Effectiveness 83 - 93 dB

@Frequency 1.00e+9 Hz
83 - 93 dB

@Frequency 1.00e+9 Hz
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone..