Parker Chomerics MESH STRIP™ (all metal) Wire Mesh EMI Gasket Selection Guide

Category Metal
Manufacturer Parker Chomerics
Trade Name MESH STRIP™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics MESH STRIP™ (all metal) Wire Mesh EMI Gasket Selection Guide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by Chomerics
Electrical Properties Metric English Comments
Shielding Effectiveness 20 - 30 dB

@Frequency 14000 Hz
20 - 30 dB

@Frequency 14000 Hz
83 - 93 dB

@Frequency 1.00e+9 Hz
83 - 93 dB

@Frequency 1.00e+9 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Descriptive Properties Value Comments
Maximum Joint Unevenness, % of Gasket Height 20-25%
Class C- Completely Interchangeable
25-30%
Class B- Open-Close in Same Position
30-40%
Class A- Permanently Closed