Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 35.0 - 96.0 dB | 35.0 - 96.0 dB | Average value: 70.3 dB Grade Count:5 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |