Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP310E Cotton Fabric Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP342 Cotton Fabric Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP691 Paper Base Laminate Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0... |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.57 mm |
300 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Dielectric Strength | 11.8 kV/mm @Frequency 60.0 Hz |
300 kV/in @Frequency 60.0 Hz |
Wet, step-by-step; ASTM D149 |
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole RX 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Dielectric Strength | 11.8 kV/mm @Thickness 1.91 mm |
300 kV/in @Thickness 0.0750 in |
Environmental Sealing Compound; ASTM D149 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Dielectric Strength | 11.8 kV/mm @Temperature 23.0 °C |
300 kV/in @Temperature 73.4 °F |
ASTM D149-97A |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 11.8 kV/mm @Temperature 23.0 °C |
300 kV/in @Temperature 73.4 °F |
ASTM D149-97A |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 11.8 kV/mm @Temperature 23.0 °C |
300 kV/in @Temperature 73.4 °F |
ASTM D149-97A |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 11.8 kV/mm @Temperature 23.0 °C |
300 kV/in @Temperature 73.4 °F |
ASTM D149-97A |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 11.8 kV/mm @Frequency 60.0 Hz |
300 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |